Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL GTX RNX130 PPE+PS+PA

Category Polymer , Thermoplastic , Nylon , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX RNX130 PPE+PS+PA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% glass reinforced PPE+PS+PA alloy for automotive and nonautomotive applications. Recycle grade in black/gray only.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 138 MPa
20000 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 138 MPa
20000 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
Type I, 5 mm/min; ASTM D638
Flexural Strength 186 MPa
27000 psi
1.3 mm/min, 50 mm span; ASTM D790
186 MPa
27000 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 7.86 GPa
1140 ksi
2.6 mm/min, 100 mm span; ASTM D790
8.13 GPa
1180 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.420 J/cm
0.787 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
Dart Drop, Total Energy 6.00 J

@Temperature 23.0 °C
4.43 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 251 °C

@Thickness 3.20 mm
484 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 229 °C

@Thickness 3.20 mm
444 °F

@Thickness 0.126 in
unannealed; ASTM D648