Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Valox®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Moisture Absorption 0.0800 %
0.0800 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.080 %
0.080 %
ISO 62
Linear Mold Shrinkage, Flow 0.011 - 0.014 cm/cm

@Thickness 3.20 mm
0.011 - 0.014 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 9.3 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.3 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Melt Index of Compound 7.0 g/10 min

@Load 5.00 kg,
Temperature 250 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
50 mm/min; ISO 527
41.0 MPa
5950 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 48.0 MPa
6960 psi
Type I, 50 mm/min; ASTM D638
48.0 MPa
6960 psi
50 mm/min; ISO 527
Elongation at Break 74 %
74 %
Type I, 50 mm/min; ASTM D638
74.8 %
74.8 %
50 mm/min; ISO 527
Elongation at Yield 4.6 %
4.6 %
50 mm/min; ISO 527
4.9 %
4.9 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 2.00 GPa
290 ksi
5 mm/min; ASTM D638
2.19 GPa
318 ksi
1 mm/min; ISO 527
Flexural Yield Strength 73.0 MPa
10600 psi
2 mm/min; ISO 178
75.0 MPa
10900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min; ISO 178
2.10 GPa
305 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
1.67 J/cm

@Temperature -30.0 °C
3.13 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
10.0 kJ/m²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 3.40 J/cm²
16.2 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 81.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
81.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 97.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
54.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
97.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
54.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 122 °C
252 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
127 °C

@Thickness 3.20 mm
261 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
88.0 °C

@Thickness 3.20 mm
190 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 130 °C
266 °F
Rate B/50; ASTM D1525
130 °C
266 °F
Rate B/50; ISO 306
133 °C
271 °F
Rate B/120; ISO 306
UL RTI, Electrical 120 °C
248 °F
UL 746B
UL RTI, Mechanical with Impact 120 °C
248 °F
UL 746B
UL RTI, Mechanical without Impact 140 °C
284 °F
UL 746B
Flammability, UL94 V-0

@Thickness 0.630 mm
V-0

@Thickness 0.0248 in
UL 94 by SABIC-IP
5VA

@Thickness 3.00 mm
5VA

@Thickness 0.118 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Arc Resistance 60 - 120 sec
60 - 120 sec
UL 746A
Comparative Tracking Index 250 - 400 V
250 - 400 V
UL 746A
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcs
15 - 30 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min
>= 5.91 in/min
UL 746A
Users viewing this material also viewed the following: