Material Notes:
Product Description: PP 502P is intended for producing low denier stretched tapes with the following features:Consistent processabilityGood processability at high line speedsLow water carry overGood mechanical propertiesTypical Applications: PP 502P can be used for producing woven bags, carpet backing and concrete reinforcements.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 4.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D785
Tensile Strength, Yield 33.0 MPa
4790 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus, 1% Secant 1450 MPa
210000 psi
ASTM D790A
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Vicat Softening Point 155 °C
311 °F
ASTM D1525B
Processing Properties Metric English Comments
Processing Temperature 235 - 250 °C
455 - 482 °F
Barrel Temperature