SCG Chemicals EL-Leneâ„¢ L1810FI Linear Low Density Polyethylene Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer SCG Chemicals Co.
Trade Name EL-Lene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SCG Chemicals EL-Leneâ„¢ L1810FI Linear Low Density Polyethylene Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Characteristics:High gloss and clarityContains 3200 ppm slip agent and 2400 ppm antiblocking agentRecommended Applications:Water-quench blown film for general purpose bags such as vegetable or fruit packagingInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.919 g/cc
0.919 g/cc
ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour

@Temperature 50.0 °C
>= 1000 hour

@Temperature 122 °F
F50, 25% Igepal; ASTM D1639
Thickness 38.0 microns
1.50 mil
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 14.0 MPa
2030 psi
ASTM D882
Film Tensile Strength at Yield, TD 10.0 MPa
1450 psi
ASTM D882
Film Elongation at Break, MD 1050 %
1050 %
ASTM D882
Film Elongation at Break, TD 810 %
810 %
ASTM D882
Secant Modulus, MD 0.260 GPa
37.7 ksi
ASTM D882
Secant Modulus, TD 0.270 GPa
39.2 ksi
ASTM D882
Elmendorf Tear Strength, MD 5.71 g/micron
145 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 14.6 g/micron
370 g/mil
ASTM D1922
Dart Drop 3.40 g/micron
86.4 g/mil
ASTM D1709
Dart Drop Test 130 g
0.287 lb
ASTM D1709
Film Tensile Strength at Break, MD 46.0 MPa
6670 psi
ASTM D882
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 122 °C
252 °F
ASTM D2117
Vicat Softening Point 102 °C
216 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Optical Properties Metric English Comments
Haze 17 %
17 %
ASTM D1003
Gloss 45 %
45 %
ASTM D2457
Users viewing this material also viewed the following: