Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SCG Chemicals EL-Leneâ„¢ M70 Butene (C4) Rotational Molding Resin

Category Polymer , Thermoplastic
Manufacturer SCG Chemicals Co.
Trade Name EL-Lene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SCG Chemicals EL-Leneâ„¢ M70 Butene (C4) Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Color compound resin available in pellet / powder formKey Characteristics:High flowFast cycle timesExcellent surface finishingTypical Applications: Complex/Intricate products, high volume/short cycle time products, such as flower pots, dolls, display stands, and decorative itemsInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.935 g/cc
0.935 g/cc
ASTM D1505
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D368
Flexural Modulus 0.650 GPa
94.3 ksi
ASTM D790
Dart Drop Total Energy 2.00 J/cm

@Thickness 5.00 mm,
Temperature -40.0 °C
0.00375 ft-lb/mil

@Thickness 0.197 in,
Temperature -40.0 °F
ARM Method
Thermal Properties Metric English Comments
Melting Point 124 °C
255 °F
ASTM D2117
Crystallization Temperature 110 °C
230 °F
ASTM D2117
Descriptive Properties Value Comments
Food Contact Approved FDA
Heavy Metal Free (Base Resin) Yes
Peak Internal Air Temperature 180°C
TPE Method
Shrinkage Level small
TPE Method
UV Stabilizer UV-8 & Low UV
ASTM G155
Users viewing this material also viewed the following: