Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SIDPEC EGYPTENE® HD 5218 EA HDPE Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer SIDPEC (Sidi Kerir Petrochemicals Co.)
Trade Name EGYPTENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SIDPEC EGYPTENE® HD 5218 EA HDPE Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:House waresThin-walled food containersPET bottle base cupInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ISO 1872/1
Melt Flow 18 g/10 min

@Load 2.16 kg
18 g/10 min

@Load 4.76 lb
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
BP 13B/1
Elongation at Break >= 1000 %
>= 1000 %
BP 13B/1
Flexural Modulus 1.05 GPa
152 ksi
ISO 178-1975
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 123 °C
253 °F
ISO 306