Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Aluzink 280A YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is .. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Aluzink B420A Metal-coated Mild Steel Metal-coated Mild SteelComments: Aluzink - Aluminum-zinc coated sheet. Property values are for thicknesses 0.4 - 2.00 mm. Iron content is approximate - exact composition is not reported by the manu.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Docol® 1000 DL High-strength Steel In course of development.Data provided by SSAB Tunnplat. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Docol® 1400 DP High-strength Steel The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel .. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Docol® 4D Deep-drawing Steel Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Docol® 600DP High-strength Steel High-strength SteelComments: Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Docol® DC04 (Fe P04) Deep-drawing Steel Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Dogal 420YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Dogal B500 Metal-coated Mild Steel Metal-coated Mild SteelComments: Dogal - Hotdipped-galvanized sheet. Property values are for thicknesses 0.5 - 2.5 mm. Iron content is approximate - exact composition is not reported by the manufac.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Domex® 014 BOR Oil quenched Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Domex® 220YP Cold-forming Steel, HSLA Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex®.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Domex® 420XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Domex® 500MC HSLA Steel HSLA SteelCharacteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum .. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Domex® 740XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Density | 7.87 g/cc @Temperature 20.0 °C |
0.284 lb/in³ @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Grade 45 Type 1 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Density | 7.87 g/cc @Temperature 20.0 °C |
0.284 lb/in³ @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Grade 55 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ASTM A 424 Type II, VIT-PLUS® DS Enameling Carbon Steel VIT-PLUS is a controlled chemistry, non-decarburized steel designed to replace certain types of ingot products. It has good strength after fire properties. It is not recommended for direct-on cove.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ASTM A 607 Class 1 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ASTM A 607 Class 2 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel CL 1/ SAE J1392 045 XLK, Grade 45 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel Full Hard Only, Grade 80 Cold Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel Type 1 & 2, Grade 33 Cold Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade Interstitial Free (I-F) steels are made by adding titanium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Commercial Steel (CS Type B), Standard Grade May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Commercial Steel (FS Type B), Standard Grade May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
ATI Allegheny Ludlum AL 418™ Special (Greek Ascoloy) Martensitic Stainless Steel Uses include engine braces, turbine exhaust components, exhaust struts, stiffeners, and ducts.Information provided by Allegheny Ludlum |
|||
Density | 7.87 g/cc @Temperature 20.0 °C |
0.284 lb/in³ @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Grade 40 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel SAE J1392, Grade 55F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) AK Steel Formable Grade - F indicates inclusion controlled low alloy.Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Steel, Bake Hardenable (BH 210) Brake Hardenable steels offer good formability and an increase in strength after paint bake.Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Bake Hardenable (BH 250) Information provided by AK Steel |