Shin-Etsu Silicones KE-1223 Silicone, Potting/Encapsulation RTV

Category Polymer , Thermoset , Silicone , Silicone, RTV, Encapsulation Grade
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KE-1223 Silicone, Potting/Encapsulation RTV.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 2.24 g/cc
2.24 g/cc
Viscosity 9000 cP
9000 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
Tensile Strength 2.00 MPa
290 psi
Thermal Properties Metric English Comments
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Strength 23.0 kV/mm
584 kV/in
Dissipation Factor 0.0020

@Frequency 50.0 Hz
0.0020

@Frequency 50.0 Hz
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 100 °C
1.00 hour

@Temperature 212 °F
Descriptive Properties Value Comments
Colors White
Mix Ratio By Weight 100:02