Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 23.0 kV/mm | 584 kV/in | |
Plastcom SLOVASTER® B1 BT PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
ASTM D149 |
Nilit Nilitop BT G6 FR C3 is a 30% Glass Fiber Reinforced, Flame Retardant PBT Description: Nilitop BT G6 FR C3 is a 30% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 3.20 mm |
584 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 3.20 mm |
584 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | IEC 60243-1 |
Celanese Celanex® 3100-2 PBT, 7.5% Glass Reinforced
(Unverified Data**) Celanex 3100 is a general purpose, 7.5% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3100 is a high flow material.7.5% glass-f.. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | |
Plastcom SLOVASTER® B FRN 3 LS PBT, flame retarder, light stable FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | |
Plastcom SLOVASTER® B FRN 3 PBT, flame retarder FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | IEC 60243-1 |
DSM Arnite® D00 301 PET (European Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
IEC 243-1 |
LATI LATAN 13 G/303 30% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | ASTM D149 |
Kingfa FW-650 Flame Retardant ABS Features:Weather resistanceSuper high impact resistanceApplications:Injection moldingSwitchSocketInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | ASTM D149 |
Kingfa H-12 Modified ABS Features:UL94 HB @ 1.6-3.0mmHigh toughnessHeat resistanceApplications:Automobile exterior trimAutomobile interior trimPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | ASTM D149 |
Kingfa HP-126 Modified ABS Features:UL94 HB @ 1.6-3.0mmHigh impact resistanceHigh flowApplications:LCD cabinetLarge thin-wall partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.00 mm |
584 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical Lupox® GP1000W PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCD861A PPE-TPE (Asia Pacific) Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCP921A PPE-TPE Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Dielectric Strength | 23.0 kV/mm | 583 kV/in | |
Saint-Gobain CHR® 23816 Glass-Silicone Backing Silicone Adhesive Pressure Sensitive Tape Description: Silicone glass provides temperature resistance from -85°F to +500°F (-62°C to +260°C) and exceptional tensile strength and abrasion resistance. Applications include thermal .. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | ASTM D149 |
Samyang Triloy® 120H PC/ABS alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 3.20 mm |
584 kV/in @Thickness 0.126 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.59 mm |
585 kV/in @Thickness 0.0625 in |
|
Cytec EN-2532 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | IEC 60243 |
Azoty Tarnow™ TARNOFORM 300 TF4 POM Tribological modified grade with addition of 20% PTFE, with very low coefficient of friction and wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | ASTM D149 |
Asahi Glass AFLAS® 100S TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.00 mm |
584 kV/in @Thickness 0.0394 in |
ASTM D149 |
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Chemical Industry KAIFA® 201-G20R PBT Resin 15% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Chemical Industry KAIFA® HN201-G20 PA6 Resin 20% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | IEC 60243-1 |
Celanese CELANEX 2104UV PBT, UV Resistant Celanex 2104UV is an unreiforced, impact modified, UV stabilized PBT designed for outdoor agricultural, industrial and automotive applications. Celanex 2104UV is suitable for injection molding appli.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.00 mm |
584 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
IEC 243-1 |
LATI LASTIROL TR G/10-V1 10% Glass Fiber Reinforced Polystyrene (PS) (UL94 V-1)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | IEC 60243-1 |
Lanxess Pocan® S 7020 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified |