Shin-Etsu Silicones LIMSâ„¢ KE1950-35A/B Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Shin-Etsu Silicones
Trade Name LIMS™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones LIMSâ„¢ KE1950-35A/B Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Viscosity 500000 cP
500000 cP
A
500000 cP
500000 cP
B
Linear Mold Shrinkage 0.022 cm/cm
0.022 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 36
36
Tensile Strength 9.80 MPa
1420 psi
Elongation at Yield 700 %
700 %
100% Modulus 0.000745 GPa
0.108 ksi
Tear Strength 30.0 kN/m
171 pli
Compression Set 4.0 %

@Temperature 200 °C,
Time 14400 sec
4.0 %

@Temperature 392 °F,
Time 4.00 hour
36 %

@Temperature 150 °C,
Time 3600 sec
36 %

@Temperature 302 °F,
Time 1.00 hour
Processing Properties Metric English Comments
Cure Time 5.00 min

@Temperature 120 °C
0.0833 hour

@Temperature 248 °F
Press Cure
60.0 min

@Temperature 150 °C
1.00 hour

@Temperature 302 °F
Post Cure
Descriptive Properties Value Comments
Appearance Translucent
Cure Rate 34
T10 (302°F, ODR)
40
T90 (302°F, ODR)
Regulatory Testing Class VI, FDA