Sibur 15303-003 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Sibur
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur 15303-003 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For production of films and film articles, including thermoset films, thin films, food contact grade films (including tight packing), general-purpose films, and bags.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
GOST 15139
Environmental Stress Crack Resistance 500 hour
500 hour
GOST 13518
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
GOST 11645
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.7 MPa
1990 psi
500 mm/min; GOST 11262
Tensile Strength, Yield 9.80 MPa
1420 psi
500 mm/min; GOST 11262
Elongation at Break 600 %
600 %
500 mm/min; GOST 11262
Descriptive Properties Value Comments
Extractable Substances 0.4 wt%
GOST 26393
Odor and taste of aqueous extracts, 1 point
GOST 22648
Process Film
Region Europe/Turkey
Bamberger Polymers Distribution