Solvay Chemicals NOCOLOK® Li Flux Drystatic

Category Ceramic
Manufacturer Solvay Chemicals
Trade Name NOCOLOK®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals NOCOLOK® Li Flux Drystatic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flux for aluminum brazing with further reduced residue solubility and improved corrosion characteristics and using electrostatic/dry powder coating.HS No.: 38109090 /CAS-No.: 60304-36-1 and 13821-20-0Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical AppliancesInformation provided by Solvay
Physical Properties Metric English Comments
Bulk Density 0.600 - 0.900 g/cc
0.0217 - 0.0325 lb/in³
Density 2.80 - 3.00 g/cc

@Temperature 20.0 °C
0.101 - 0.108 lb/in³

@Temperature 68.0 °F
Solubility in Water 0.45 %
0.45 %
Thermal Properties Metric English Comments
Melting Point 569 - 577 °C
1060 - 1070 °F
Descriptive Properties Value Comments
Appearance White powder