Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.80 g/cc | 0.101 lb/in³ | |
Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite Formerly known as grade MM 1100. Synthetic mica filler. Does not burn. Excellent radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating m.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Rogers Corporation RO3010 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits: |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Pyrotek Pyrocast ZEAL Refractory Shapes Aggregate Base: MulliteApplicationsDoor sill Furnace ramp Crucible bottom / lining Information provided by Pyrotek. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Apparent |
Gouda Vuurvast AK 85 KM Dense Refractory Brick Description: This brick based on mullite and corundum, is characterized by a very low porosity, high slag resistance, low creep and very good thermal shock resistance.Remarks: This data represents a.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Schott GM27884 Dental Glass Remarks: Ba-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SC.. |
|||
Density | 2.80 g/cc @Temperature 20.0 °C |
0.101 lb/in³ @Temperature 68.0 °F |
|
Solvay Chemicals KaCeFlux Potassium Fluoroaluminate Standard flux for brazing aluminum.HS No.: 3810100000 /CAS-No.: 60304-36-1 and 14484-69-6Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electri.. |
|||
Density | 2.80 - 3.00 g/cc @Temperature 20.0 °C |
0.101 - 0.108 lb/in³ @Temperature 68.0 °F |
|
Solvay Chemicals NOCOLOK® Cs Flux Flux for brazing magnesium aluminum alloysHS No.: 38109090/CAS-No.: 60304-36-1 and 138577-01-2Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Elect.. |
|||
Density | 2.80 g/cc @Temperature 20.0 °C |
0.101 lb/in³ @Temperature 68.0 °F |
|
Solvay Chemicals NOCOLOK® Flux Drystatic Potassium Fluoroaluminate Flux using electrostatic/dry powder coating. Classifications: HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & .. |
|||
Density | 2.80 - 3.00 g/cc @Temperature 20.0 °C |
0.101 - 0.108 lb/in³ @Temperature 68.0 °F |
|
Solvay Chemicals NOCOLOK® Flux P2 Potassium Fluoroaluminate Mixtures of NOCOLOK® Flux P2 with NOCOLOK® Flux allow for gradual viscosity adjustments in suspensions to suit specific process conditions.HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automoti.. |
|||
Density | 2.80 g/cc @Temperature 20.0 °C |
0.101 lb/in³ @Temperature 68.0 °F |
|
Solvay Chemicals NOCOLOK® Flux Potassium Fluoroaluminate A high quality fluxing agent for brazing aluminum components. Classifications: HS No.: 38109090/CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration .. |
|||
Density | 2.80 - 3.00 g/cc @Temperature 20.0 °C |
0.101 - 0.108 lb/in³ @Temperature 68.0 °F |
|
Solvay Chemicals NOCOLOK® Li Flux Flux for aluminum brazing with further reduced residue solubility and improved corrosion characteristics.HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air.. |
|||
Density | 2.80 - 3.00 g/cc @Temperature 20.0 °C |
0.101 - 0.108 lb/in³ @Temperature 68.0 °F |
|
Solvay Chemicals NOCOLOK® Li Flux Drystatic Flux for aluminum brazing with further reduced residue solubility and improved corrosion characteristics and using electrostatic/dry powder coating.HS No.: 38109090 /CAS-No.: 60304-36-1 and 13821-.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec 665 Steatite, MgO•SiO2 Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. 665 L533C has low dielectric loss. It makes exc.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Frequenta® Steatite Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. Frequenta® has low dielectric loss, but has be.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Vista Metals Duramold-2™ Cast Aluminum Mold Plate Used for molds for the automotive industry, blow molds, structural foam molds, rubber molds, low pressure injection molds, Thermoforming molds, R.I.M. and R.T.M. molding.Features: Excellent Machinab.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | ASTM C20 |
CoorsTek Mullite, S2 Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | ASTM C20 |
CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide Thermal Shock Delta Tc = 600°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Du-Co Ceramics DC-200-L-5 Fosterite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
COI Ceramics Nextel™ AS-N650 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon CP-594CX Bulk Compound Product Use: Electrically insulating electronic adhesive. Bonds without primer.Appearance: Gray, high viscosity gumUL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but .. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
ALIMEX ACP 6000 Aluminum Cast Plate Aluminum cast plate ACP 6000 is a 7xxx series alloy surface-machined plate. This type of alloy ensures excellent machinability characteristics and adequate tensile strength. Thickness, flatness and .. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon Thermabond® 48A43X008 0.008"(0.203 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® Electrically insulating, thermally conductive, thermal interface material (TIM).Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cu.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon Thermabond® 99A50X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Alpase M-1™ Aluminum Mold Plate M-1™ features and benefits include: Dimensional stability, fully weldable, anodizable, consistent hardness - regardless of size, can be nickel plated, good machinability, no heat treatment required.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | |
Alpase M-5™ Aluminum Mold Plate Excellent weldabilitySurface Condition - Machined top and bottom to reduce costly handling and machining stepsDimensional Stability - High dimensional stability during and after machiningPolishing -.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon R37480X008 0.008" (0.203 mm) Uncured Silicone Rubber with Substrate: PTFE Coated Fiberglass Substrate Description: Primerless Thermabond® electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substra.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon R37622X008 0.008" (0.203 mm) Cured Silicone Rubber with Release PET Carrier Description: Thermabond® electrically insulating, thermally conductive, thermal interface materialDesign/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fiber.. |
|||
Density | 2.80 g/cc | 0.101 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber Description: Thermabond® electrically insulating, thermally conductive, thermal interface material. Design/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fib.. |