Physical Properties Metric English Comments
Density 2.30 - 3.00 g/cc
0.0831 - 0.108 lb/in³
ASTM B417
H.C. Starck Amperit® 582.072 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)
Density 2.30 - 3.00 g/cc
0.0831 - 0.108 lb/in³
ASTM B212
H.C. Starck Amperit® 586.054 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)
Density 2.30 - 3.00 g/cc
0.0831 - 0.108 lb/in³
ASTM B212
H.C. Starck Amperit® 586.1 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)
Density 2.30 - 3.00 g/cc
0.0831 - 0.108 lb/in³
ASTM B212
H.C. Starck Amperit® 588.074 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 45/15 µm
Density 2.30 - 3.00 g/cc
0.0831 - 0.108 lb/in³
ASTM B212
H.C. Starck Amperit® 599.063 Agglomerated Sintered Molybdenum Carbide (Cr2O3)
Density 2.80 - 3.00 g/cc

@Temperature 20.0 °C
0.101 - 0.108 lb/in³

@Temperature 68.0 °F
Solvay Chemicals NOCOLOK® Cs Flux
Flux for brazing magnesium aluminum alloysHS No.: 38109090/CAS-No.: 60304-36-1 and 138577-01-2Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Elect..
Density 2.80 - 3.00 g/cc

@Temperature 20.0 °C
0.101 - 0.108 lb/in³

@Temperature 68.0 °F
Solvay Chemicals NOCOLOK® Flux P2 Potassium Fluoroaluminate
Mixtures of NOCOLOK® Flux P2 with NOCOLOK® Flux allow for gradual viscosity adjustments in suspensions to suit specific process conditions.HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automoti..
Density 2.80 - 3.00 g/cc

@Temperature 20.0 °C
0.101 - 0.108 lb/in³

@Temperature 68.0 °F
Solvay Chemicals NOCOLOK® Li Flux
Flux for aluminum brazing with further reduced residue solubility and improved corrosion characteristics.HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air..
Density 2.80 - 3.00 g/cc

@Temperature 20.0 °C
0.101 - 0.108 lb/in³

@Temperature 68.0 °F
Solvay Chemicals NOCOLOK® Li Flux Drystatic
Flux for aluminum brazing with further reduced residue solubility and improved corrosion characteristics and using electrostatic/dry powder coating.HS No.: 38109090 /CAS-No.: 60304-36-1 and 13821-..
Density 2.30 - 3.00 g/cc
0.0831 - 0.108 lb/in³
ASTM B212
H.C. Starck Amperit® 584.1 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr)
Density 2.30 - 3.00 g/cc
0.0831 - 0.108 lb/in³
ASTM B212
H.C. Starck Amperit® 588.088 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 53/20 µm
Density 2.30 - 3.00 g/cc
0.0831 - 0.108 lb/in³
ASTM B212
H.C. Starck Amperit® 584.054 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr)