Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA), 22% Glass Fiber

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 20% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA), 22% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in water-cooled molds. This resin exhibits high heat resistance, high strength and stiffness over a broad temperature range, low moisture absorption, excellent chemical resistance and excellent electrical properties. Features: Fast Molding Cycle; Good Chemical Resistance; Good Color Stability; High Reflectivity; High Stiffness; Light Stabilized; Low Moisture AbsorptionUses: Automotive Applications; Automotive ElectronicsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Additional Properties: Optical Reflectivity - ASTM E1331 (460 nm): > 90 %; Optical Reflectivity - ASTM E1331 (540 nm): > 90 %; Optical Reflectivity - ASTM E1331 (615 nm): > 90 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
Filler Content 22 %
22 %
Glass Fiber
Water Absorption 0.19 %

@Time 86400 sec
0.19 %

@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 124
124
ASTM D785
Tensile Strength 104 MPa
15100 psi
ASTM D638
Elongation at Break 1.2 %
1.2 %
ASTM D638
Tensile Modulus 9.10 GPa
1320 ksi
ASTM D638
Flexural Strength 165 MPa
23900 psi
ASTM D790
Flexural Modulus 8.10 GPa
1170 ksi
ASTM D790
Izod Impact, Notched 0.180 J/cm
0.337 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 150 - 250 °C
10.6 µin/in-°F

@Temperature 302 - 482 °F
2
25.0 µm/m-°C

@Temperature 0.000 - 100 °C
13.9 µin/in-°F

@Temperature 32.0 - 212 °F
2
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 0.000 - 100 °C
53.3 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM E228
150 µm/m-°C

@Temperature 100 - 250 °C
83.3 µin/in-°F

@Temperature 212 - 482 °F
ASTM E228
Melting Point 323 °C
613 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
554 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 318 - 324 °C
604 - 615 °F
Middle Barrel Temperature 318 - 324 °C
604 - 615 °F
Front Barrel Temperature 327 - 332 °C
621 - 630 °F
Melt Temperature 329 - 343 °C
624 - 649 °F
Mold Temperature 65.0 - 93.0 °C
149 - 199 °F
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Moisture Content 0.030 - 0.060 %
0.030 - 0.060 %
Suggested Max
Descriptive Properties Value Comments
Additive UV Stabilizer
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color White
Form Pellets
Processing Technique Water-Heated Mold Injection Molding
RoHS Compliance RoHS Compliant