Material Notes:
Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is available in black and natural colors.Benefits: Due to its outstanding flow characteristics, the product shows exceptional processing behavior and excellent surface aspect of the finished part.Available in: Europe, Latin America and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: The product is particularly suitable for all applications where a high rigidity is required: typically structural parts or brackets for the automotive industry. Its high mechanical performance allows that product to be an alternative to metal parts.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ISO 1183/A
Water Absorption 0.60 %

@Temperature 23.0 °C,
Time 86400 sec
0.60 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0034 cm/cm
0.0034 in/in
Linear Mold Shrinkage, Transverse 0.0042 cm/cm
0.0042 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 255 MPa
37000 psi
ISO 527 Type 1A
Tensile Stress 100 MPa

@Strain 1.00 %
14500 psi

@Strain 1.00 %
145 MPa

@Strain 2.00 %
21000 psi

@Strain 2.00 %
180 MPa

@Strain 3.00 %
26100 psi

@Strain 3.00 %
Elongation at Break 2.5 %
2.5 %
ISO 527 Type 1A
Tensile Modulus 17.0 GPa
2470 ksi
ISO 527 Type 1A
Flexural Strength 380 MPa
55100 psi
ISO 178
Flexural Modulus 15.0 GPa
2180 ksi
ISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180/1eA
Izod Impact, Unnotched (ISO) 88.0 kJ/m²
41.9 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 10.0 J/cm²
47.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 264 °C
507 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 256 °C
493 °F
ISO 75/Af
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
1210
Glow Wire Test 650 °C

@Thickness 0.800 mm
1200 °F

@Thickness 0.0315 in
ISO 60695-2-12
675 °C

@Thickness 0.800 mm
1250 °F

@Thickness 0.0315 in
ignition temperature; ISO 60695-2-12
Processing Properties Metric English Comments
Feed Temperature 260 - 270 °C
500 - 518 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 270-280°C
Mixing Zone 280-290°C
Users viewing this material also viewed the following: