Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 650 °C @Thickness 3.20 mm |
1200 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Glow Wire Test | 650 °C @Thickness 0.800 mm |
1200 °F @Thickness 0.0315 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Glow Wire Test | 650 °C @Thickness 0.800 mm |
1200 °F @Thickness 0.0315 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66 Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app.. |
|||
Glow Wire Test | 650 °C @Thickness 3.20 mm |
1200 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It .. |
|||
Glow Wire Test | 650 °C @Thickness 0.800 mm |
1200 °F @Thickness 0.0315 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid B3 H G8 40% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G8 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key character.. |
|||
Glow Wire Test | 650 °C @Thickness 0.800 mm |
1200 °F @Thickness 0.0315 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid A3 H G6 General Purpose 30% Glass Reinforced PA66 Description: Nilamid A3 H G6 is a general purpose 30% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi.. |
|||
Glow Wire Test | 650 °C @Thickness 0.800 mm |
1200 °F @Thickness 0.0315 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid A3 H G7 General Purpose 35% Glass Reinforced PA66 Description: Nilamid A3 H G7 is a general purpose 35% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi.. |
|||
Glow Wire Test | 650 °C @Thickness 3.20 mm |
1200 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid A3 H6 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H6 G6 is a 30% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Glow Wire Test | 650 °C @Thickness 0.800 mm |
1200 °F @Thickness 0.0315 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid A3 H6 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H6 G6 is a 30% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Glow Wire Test | 650 °C @Thickness 3.20 mm |
1200 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G10 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key characte.. |
|||
Glow Wire Test | 650 °C @Thickness 3.20 mm |
1200 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid.. |
|||
Glow Wire Test | 650 °C @Thickness 0.800 mm |
1200 °F @Thickness 0.0315 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,.. |
|||
Glow Wire Test | 650 °C @Thickness 3.20 mm |
1200 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,.. |
|||
Glow Wire Test | 650 °C @Thickness 1.50 mm |
1200 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific) DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r.. |
|||
Glow Wire Test | 650 °C @Diameter 0.800 mm |
1200 °F @Diameter 0.0315 in |
IEC 60695-2-12 |
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers PA 66, 30% glass fibers, injection molding, heat-ageing stabilized |
|||
Glow Wire Test | 650 °C @Thickness 0.800 mm |
1200 °F @Thickness 0.0315 in |
ISO 60695-2-12 |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
ISO 60695-2-12 |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Glow Wire Test | 650 °C @Thickness 0.800 mm |
1200 °F @Thickness 0.0315 in |
ISO 60695-2-12 |
Solvay TECHNYL® A 216 PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert.. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
ISO 60695-2-12 |
Solvay TECHNYL® A 216 PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert.. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
Ignition Temperature; ISO 60695-2-13 |
Solvay TECHNYL® A 216 PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert.. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
ISO 60695-2-12 |
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, DRY Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent .. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
ISO 60695-2-12 |
Solvay TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, DRY Description: Polyamide PA66, reinforced with 20% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V20 is used in all sectors of industry.. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
ISO 60695-2-12 |
Solvay TECHNYL® A 216 NATURAL FA PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 Natural FA offers all of the primary properties of unreinf.. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
ISO 60695-2-12 |
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is .. |
|||
Glow Wire Test | 650 - 750 °C @Thickness 2.00 mm |
1200 - 1380 °F @Thickness 0.0787 in |
VDE 0471/P2-4, IEC 695 |
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
VDE 0471/P2-4, IEC 695 |
EPICHEM Epiryl B PPO Polyphenylene oxide |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
Glow-Wire Ignition; IEC 60695-2-13 |
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Glow Wire Test | 650 °C @Thickness 3.00 mm |
1200 °F @Thickness 0.118 in |
DAM; Flammability Index; IEC 60695-2-12 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
Glow Wire Test | 650 °C @Thickness 0.800 mm |
1200 °F @Thickness 0.0315 in |
flammability index; IEC-60695-2-12 |
Solvay TECHNYL® 2411GF6 PA66, 30% glass fiber, DRY Description: Polyamid 66, 30% glass fiber reinforce, for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2411GF6 used in all sectors of industry, offering an excellent com.. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
ignition temperature; IEC-60695-2-13 |
Solvay TECHNYL® 2411GF6 PA66, 30% glass fiber, DRY Description: Polyamid 66, 30% glass fiber reinforce, for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2411GF6 used in all sectors of industry, offering an excellent com.. |