Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 60% Glass Fiber Filled
Manufacturer Solvay
Trade Name TECHNYLSTAR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applications: TECHNYLSTAR TM SX 216 V60 is suitable for all applications where a high rigidity is required. Due to its outstanding flow properties, the material easily fills the mould and the surface aspect of the finished part is excellent. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 165 MPa
23900 psi
ISO 527 Type 1A
Elongation at Break 3.7 %
3.7 %
ISO 527 Type 1A
Tensile Modulus 15.5 GPa
2250 ksi
ISO 527 Type 1A
Flexural Modulus 13.2 GPa
1910 ksi
ISO 178
Izod Impact, Notched (ISO) 22.0 kJ/m²
10.5 ft-lb/in²
ISO 180/1eA
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 9.50 J/cm²
45.2 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Users viewing this material also viewed the following: