Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech Royalite R522 PVC Alloy Aircraft Grade Sheet

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Sheet Grade
Manufacturer Spartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Royalite R522 PVC Alloy Aircraft Grade Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Aircraft Grade SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.27 - 1.30 g/cc
1.27 - 1.30 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Flexural Yield Strength 66.2 MPa
9600 psi
ASTM D790
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
73°F; ASTM D256
Impact Test 50.2 J

@Temperature 22.8 °C
37.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 81.0 µm/m-°C

@Temperature 20.0 °C
45.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ASTM D648
Descriptive Properties Value Comments
FAA 12 Second Vertical Burn Passes
FAR Pt 25, App F, Pt I
FAA 60 Second Vertical Burn Passes
FAR Pt 25, App F, Pt I
Flammability Passes
MVSS (Motor Vehicle Safety Standard) 302