Description: Weather Resistant SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.01 - 1.06 g/cc
1.01 - 1.06 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 91
91
ASTM D785
Tensile Strength, Yield 31.7 MPa
4600 psi
ASTM D638
Flexural Yield Strength 51.7 MPa
7500 psi
ASTM D790
Flexural Modulus 1.86 GPa
270 ksi
ASTM D790
Izod Impact, Notched 3.74 J/cm
7.00 ft-lb/in
73°F; ASTM D256
1.07 J/cm

@Temperature -28.9 °C
2.00 ft-lb/in

@Temperature -20.0 °F
ASTM D256
Impact Test 35.3 J

@Temperature 22.8 °C
26.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 75.6 - 101 µm/m-°C

@Temperature 20.0 °C
42.0 - 56.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 96.1 °C
205 °F
ASTM D648
Descriptive Properties Value Comments
Flammability Passes
MVSS (Motor Vehicle Safety Standard) 302