Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech SP-1510 Polyolefin Sheet

Category Polymer , Thermoplastic , Polyethylene (PE) , Polyolefin
Manufacturer Spartech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech SP-1510 Polyolefin Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyolefin SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D2240
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Tensile Modulus 0.827 GPa
120 ksi
ASTM D638
Flexural Modulus 1.14 GPa
165 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 126 µm/m-°C

@Temperature 20.0 °C
70.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 71.1 °C
160 °F
ASTM D648
Flammability, UL94 HB
HB