Spartech Soft Touch HDPE Polyolefin Skin/Specialty Sheet

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , Polyolefin
Manufacturer Spartech
Trade Name Soft Touch
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Soft Touch HDPE Polyolefin Skin/Specialty Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Specialty SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Flexural Yield Strength 65.5 MPa
9500 psi
ASTM D790
Flexural Modulus 1.14 GPa
165 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 126 µm/m-°C

@Temperature 20.0 °C
70.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 71.1 °C
160 °F
ASTM D648