Spartech Spectrum® S630 MDPE Polyolefin Sheet  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Spectrum® S630 MDPE Polyolefin Sheet  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell R 50
50
Tensile Strength, Ultimate 20.5 MPa
2970 psi
Machine direction
Flexural Yield Strength 26.9 MPa
3900 psi
Flexural Modulus 1.00 GPa
145 ksi
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C
111 °F