Polymer Property : Izod Impact, Unnotched = 11.5 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 6.14 J/cm
11.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP FARADEX WX94736 PBT
LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel.
Izod Impact, Unnotched 6.14 - 8.01 J/cm
11.5 - 15.0 ft-lb/in
Average value: 7.14 J/cm Grade Count:4
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Izod Impact, Unnotched 6.12 J/cm

@Temperature 23.0 °C
11.5 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Stat-kon WEF42 PET/PBT
LNP Stat-Kon WCF-1006 is a compound based on PET/PBT resin containing carbon and glass fiber reinforcements.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 6.14 J/cm
11.5 ft-lb/in
Stratasys® Ultem 9085 for Rapid Prototyping
ULTEM* 9085 is a fl ame retardant high performance thermoplastic for direct digital manufacturing and rapid prototyping. It is ideal for the transportation industry due to its high strength-to-weigh..
Izod Impact, Unnotched 6.14 J/cm
11.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP JF006 PES
LNP* THERMOCOMP* JF006 is a compound based on Polyethersulfone resin containing 30% Glass Fiber.
Izod Impact, Unnotched 6.14 J/cm
11.5 ft-lb/in
ASTM D4812
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Izod Impact, Unnotched 6.14 J/cm
11.5 ft-lb/in
ASTM D4812
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Izod Impact, Unnotched 6.14 J/cm
11.5 ft-lb/in
ASTM D4812
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Izod Impact, Unnotched 6.14 J/cm
11.5 ft-lb/in
ASTM D4812
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Izod Impact, Unnotched 6.14 J/cm
11.5 ft-lb/in
ASTM D4812
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Izod Impact, Unnotched 6.14 J/cm
11.5 ft-lb/in
ASTM D4812
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT
Information provided by A. Schulman.