Material Notes:
N,N` Ethylene Bis-stearamideSTRUKTOL® TR EBS is an exceptionally effective dispersion aid for a wide range of organic and inorganic pigments. STRUKTOL® TR EBS can be used in most polymer carrier systems.FDA Status: 175.105; 175.300; 176.170; 176.180; 177.1200; 177.1350; 177.1400; 177.2470; 177.2480
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Thermal Properties Metric English Comments
Melting Point 138 - 150 °C
280 - 302 °F
Chemical Properties Metric English Comments
Acid Value <= 10
<= 10
Processing Properties Metric English Comments
Shelf Life >= 24.0 Month
>= 24.0 Month
Descriptive Properties Value Comments
Appearance White pastille or bead