Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 140 - 150 °C | 284 - 302 °F | Melt Range for MFI=10; MQSA 111 |
Lubrizol Advanced Materials Pearlcoat® 125KW Thermoplastic Polyurethane Elastomer
(discontinued **) Pearlcoat® D125KW is a polyester-based aromatic TPU, supplied in form of white-colored pellets, combining hardness with excellent low-temperature flexibility.Applications: Pearlcoat® D125KW is us.. |
|||
Melting Point | 115 - 150 °C | 239 - 302 °F | |
M Chemical GUARD DOGâ„¢ UV119 HALS Light Stabilizer GUARD DOGâ„¢ UV119 is effective in polypropylene, polyethylene, alpha-olefin copolymers and blends with EPR, ERR, PE, EVA, EAA, EVOH and filled PP.Typical Properties:Appearance - White to light y.. |
|||
Melting Point | 140 - 150 °C | 284 - 302 °F | |
Fine Organics FINALUX CB 50 Composite Lubricant Applications: Composite lubricant with co-stabilizing properties for rigid PVC extrusion/injection molding.Information provided by Fine Organics |
|||
Melting Point | 110 - 150 °C | 230 - 302 °F | ISO 3146-C |
FKuR Kunststoff Bio-Flex® S 6540 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Melting Point | 140 - 150 °C | 284 - 302 °F | MQSA 114 |
Lubrizol Advanced Materials Pearlthane® D91F65D Thermoplastic Polyurethane Elastomer PEARLTHANE® D91F65D is an aliphatic TPU supplied in colourless natural pellets. In addition to typical TPU properties like outstanding abrasion loss, PEARLTHANE® D91F65D offers excellent colou.. |
|||
Melting Point | 138 - 150 °C | 280 - 302 °F | |
Struktol TR EBS Processing Additive, Dispersant N,N` Ethylene Bis-stearamideSTRUKTOL® TR EBS is an exceptionally effective dispersion aid for a wide range of organic and inorganic pigments. STRUKTOL® TR EBS can be used in most polymer carri.. |
|||
Melting Point | 145 - 150 °C | 293 - 302 °F | DSC; ISO 3146 |
Borealis RD735CF Polypropylene Random Copolymer RD735CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD735CF is recommended for food packaging, textile packaging .. |
|||
Melting Point | 140 - 150 °C | 284 - 302 °F | DSC |
EMS-Griltech Griltex® D 1533E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 125 - 150 °C | 257 - 302 °F | |
Indium Corp. Indalloy 203 Indium Solder Alloy Information Provided by Indium Corporation |