Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution PS 153A GPPS

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Extrusion Grade
Manufacturer Styrolution
Trade Name PS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution PS 153A GPPS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Styrolution PS 153A is an antistatic modified, general purpose polystyrene grade with a good flow characteristic.AntistaticGood flow characteristicsInformation provided by Styrolution
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ISO 294-4
Melt Flow 17 g/10 min

@Load 5.00 kg,
Temperature 200 °C
17 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO 527
Elongation at Break 1.5 %
1.5 %
ISO 527
Tensile Modulus 3.20 GPa
464 ksi
ISO 527
Flexural Strength 55.0 MPa
7980 psi
ISO 178
Charpy Impact Unnotched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359
Vicat Softening Point 85.0 °C

@Load 5.10 kg
185 °F

@Load 11.2 lb
120°C/h; ASTM D 1525
Processing Properties Metric English Comments
Melt Temperature 180 - 280 °C
356 - 536 °F
ISO 294
Users viewing this material also viewed the following: