Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.800 - 2.00 J/cm² | 3.81 - 9.52 ft-lb/in² | Average value: 1.53 J/cm² Grade Count:3 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LASTIROL R G/30 30% Glass Fiber Reinforced Polystyrene (PS)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Charpy Impact Unnotched | 0.800 - 30.0 J/cm² | 3.81 - 143 ft-lb/in² | Average value: 6.23 J/cm² Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® 2863
(discontinued **) Special grade for smart cards.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® QE 1088 FC, Injection Grade
(discontinued **) Injection molding grade, high impact, medium gloss.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholdi.. |
|||
Charpy Impact Unnotched | 0.800 - 1.10 J/cm² | 3.81 - 5.23 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group RALUPOL® 802 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up.. |
|||
Charpy Impact Unnotched | 0.800 - 1.10 J/cm² | 3.81 - 5.23 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LATILUB 95-25GR CE/10 Polysulfone Base (PSU), 25% Graphite, 10% Special Mineral Filled Self Lubricating Plastic Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Charpy Impact Unnotched | 0.800 - 3.00 J/cm² | 3.81 - 14.3 ft-lb/in² | Average value: 2.27 J/cm² Grade Count:3 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 84 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets, High Mechanical Strength
& Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, moldin.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | |
LATI Latamid 12 H 90FE03 PA 12, Heat Stabilized Polyamide 12 (PA12) based compound. Heat stabilized. Magnetizable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | |
LATI Laticonther 62 GR/50 PA 6, 50% Graphite Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL PVX516 PPE PREVEX* PVX516 resin is a high flow, non FR grade, 110 C HDT |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179-1 |
Vyncolit X655/1 Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral filled. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in particular in the ABS system.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | Notched/Unnotched not specified; ASTM DIN53453 |
Total PPC 4824WZ Polypropylene, Impact Copolymer ATOFINA 4824WZ is a nucleated impact copolymer. 4824WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. It has been formulated for excellent .. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
|
Covestro Apec® HT KU 1-9353 High-Heat Polycarbonate, UV-Stabilized Transparent and opaque shades possible, UV-stabilized.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
|
Covestro Apec® HT KU 1-9354 High-Heat Polycarbonate Only opaque colors available, flame retardant.Applications: Lighting, electrical parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and off.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
|
Covestro Apec® HT KU 1-9357/2 High-Heat Polycarbonate, 20% Glass Fiber Only opaque colors available, with 20% glass fiber reinforcement, flame retardant.Applications: Lighting, electrical parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® D 1175 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® T40H 550 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eU |
CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures PP-HT is a semi-crystalline plastic, with high acid and chemical resistance and mechanical strength. Due to its high resistance to temperature, PP-HT-plastics are often used in medical technology as.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 4010 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage
(disconti Glass fiber reinforced and inorganically filled molding compound. High heat resistance, reduced molding shrinkage, good chemical resistance and mechanical properties.Application areas: Switch housi.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-8165 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1301-8144 PPS, linear, with mineral filler Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low waterabsorbtion.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² - NB | 3.81 ft-lb/in² - NB | Average value: 10.6 J/cm² Grade Count:198 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | |
LATI Latimass 62-05 D040 PA6 Specific density compound based on Polyamide 6 (PA6). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |