Styron CALIBREâ„¢ IM 401-11 Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Styron
Trade Name CALIBRE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron CALIBREâ„¢ IM 401-11 Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Melt Flow 11 g/10 min

@Load 1.20 kg,
Temperature 300 °C
11 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Elongation at Break 130 %
130 %
ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 6.94 J/cm
13.0 ft-lb/in
0.125 in; 10 mil notch; ASTM D256
5.34 J/cm

@Temperature -30.0 °C
10.0 ft-lb/in

@Temperature -22.0 °F
0.125 in; 10 mil notch; ASTM D256
Tensile Impact Strength 630 kJ/m²
300 ft-lb/in²
ASTM D1822, Type S
Dart Drop, Total Energy 57.0 J
42.0 ft-lb
0.1 in thick, 15 mph; ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
Unannealed, 0.125 in; ASTM D648
136 °C
277 °F
annealed; ASTM D648
Vicat Softening Point 146 °C
295 °F
50°C/hr, 50N Load; ASTM D1525
Flammability, UL94 HB
HB
0.0625 in
HB
HB
0.125 in