Techmer ES HiFill® ABS GF30 IM 30% Glass Filled

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® ABS GF30 IM 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
Water Absorption 0.12 %

@Time 86400 sec
0.12 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0010 cm/cm

@Thickness 3.17 mm
0.0010 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Elongation at Break 3.3 %
3.3 %
ASTM D638
Flexural Strength 121 MPa
17500 psi
ASTM D790
Flexural Modulus 6.21 GPa
900 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm

@Thickness 3.17 mm
2.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 4.81 J/cm

@Thickness 3.17 mm
9.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 28.8 µm/m-°C
16.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
218 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm
450 kV/in
Method A (Short-Time); ASTM D149