Material Notes:
Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Heat ResistanceInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ASTM D792
Water Absorption 0.17 %

@Time 86400 sec
0.17 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 234 MPa
34000 psi
ASTM D638
Elongation at Break 2.8 %
2.8 %
ASTM D638
Flexural Strength 338 MPa
49000 psi
ASTM D790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 34.2 µm/m-°C
19.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 302 °C
575 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+15 ohm-cm
8.00e+15 ohm-cm
ASTM D257
Dielectric Strength 23.6 kV/mm
600 kV/in
Method A (Short-Time); ASTM D149