Techmer ES HiFill® PA4/6 GF30 HS NAT 30% Glass Filled (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA4/6 GF30 HS NAT 30% Glass Filled (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Water Absorption 1.5 %

@Time 86400 sec
1.5 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Yield Strength 255 MPa
37000 psi
ASTM D790
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm

@Thickness 3.17 mm
1.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 18.0 µm/m-°C
10.0 µin/in-°F
ASTM D696
Melting Point 295 °C
563 °F
Deflection Temperature at 1.8 MPa (264 psi) 291 °C
555 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Dielectric Strength 23.6 kV/mm
600 kV/in
Method A (Short-Time); ASTM D149