Techmer ES HiFill® PPA GF33 FR HS L 33% Glass Filled

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PPA GF33 FR HS L 33% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Flame Retardant and LubricatedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Water Absorption 0.18 %

@Time 86400 sec
0.18 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 165 MPa
24000 psi
ASTM D638
Elongation at Break 1.8 %
1.8 %
ASTM D638
Flexural Yield Strength 228 MPa
33000 psi
ASTM D790
Flexural Modulus 12.4 GPa
1800 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 59.4 µm/m-°C
33.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 299 °C
570 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 20.9 kV/mm
530 kV/in
Method A (Short-Time); ASTM D149