Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 59.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C7210A PC+ABS (Asia Pacific) Cycoloy* C7210A resin is talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PA6/6 IM C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Additive: Impact ModifierFeatures: Conductive and Impact ModifiedAppearance: BlackInformation provided by TP.. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6 FR IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6 FR IM 004 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6 FR NAT Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6 FR-N HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 FR IM BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedAppearance: BlackTPCI# 9993101Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GB30 FR 30% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: LubricantFeatures: Flame Retardant and LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6,6 GF NAT Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA4/6 GF50 HS BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackUL File Number: E1573.. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GB20 L 20% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GB10 L 10% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GB15 15% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 15% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GB20 L BK 20% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GB25 L BK 25% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 25% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP GB60 60% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP Cycoloy_C7210A PC+ABS LNP* Thermocomp* Cycoloy_C7210A isa a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 GL10 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Graphite Powder Lubricant(10%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 GL15 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Graphite Powder Lubricant(15%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PS 06001 Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler/Unspecified FillerReinfor.Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C @Temperature 20.0 °C |
33.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Styron Pulse® 1550 ABS + Polycarbonate, 10% Glass Reinforced PULSE® 1550 Engineering resin is a 10% glass reinforced resin which offers a superior total performance with a balance of high heat resistance, practical toughness and ease of processing.Data pro.. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6 E FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant Processing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6 FR HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PET GF/M40 BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
33.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl 731H PPE+PS High gloss, general purpose grade. 130C (266F) DTUL. UL 94 HB rated. For multiple plugs, wine filter plates, etc.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
33.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL EN265 PPE+PS Extrusion grade. 254F (123C) DTUL. UL94 V-1 rated. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Entec Hyril® GP355AS Styrene Acrylonitrile Available in North America Features: Copolymer Automotive Specifications: DELPHI M-9565-9 Color: Blue-TransparentForm: PelletsProcessing Method: ExtrusionInformation provided by Entec |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Entec Hyril® SAN500 Styrene Acrylonitrile Available in North America Features: Copolymer Form: PelletsInformation provided by Entec |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 FR IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
33.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL ENG265 PPE+PS PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a.. |