Techmer ES Plaslube® AC-81/TF/15 NAT Acetal (POM) Homopolymer

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, PTFE-Filled
Manufacturer Techmer ES
Trade Name Plaslube®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® AC-81/TF/15 NAT Acetal (POM) Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Water Absorption 0.23 %
0.23 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.020 - 0.024 cm/cm
0.020 - 0.024 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 7.5 %
7.5 %
ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
ASTM D648
Users viewing this material also viewed the following: