Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plastiblend® PA6/10 BK Nylon 610

Category Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plastiblend® PA6/10 BK Nylon 610.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Water Absorption 0.40 %

@Time 86400 sec
0.40 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D638
Elongation at Yield 100 %
100 %
ASTM D638
Flexural Yield Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Thickness 3.17 mm
0.900 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 79.2 µm/m-°C
44.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
151 °F
Unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257
Users viewing this material also viewed the following: