Material Notes:
Information provided by Technetics Group (formerly Plastomer Technologies)
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
Thickness 38.1 - 635 microns
1.50 - 25.0 mil
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 10.3 MPa
>= 1500 psi
Elongation at Break >= 70 %
>= 70 %
Descriptive Properties Value Comments
Available Colors White, Clear, Standard and Custom Colors
Laser Printable Yes
Width, in 1/4-6