Teknor Apex APEX® 1013 Polyvinyl Chloride, Semi-Rigid

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 1013 Polyvinyl Chloride, Semi-Rigid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Components Additional Information: Temperature Rating: 60°C Recognized Component, CSA C22.2 No. 0.6, CSA Flammability Classification: 0.6HB at 0.88mmInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore C 77
77
10 seconds; ASTM D2240
Tensile Strength at Break 19.3 MPa
2800 psi
ASTM D638
Elongation at Break 280 %
280 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Continuous Use; ASTM D794
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D746
UL RTI, Electrical 90.0 °C

@Thickness 0.889 mm
194 °F

@Thickness 0.0350 in
UL 746
90.0 °C

@Thickness 1.40 mm
194 °F

@Thickness 0.0551 in
UL 746
90.0 °C

@Thickness 3.00 mm
194 °F

@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 0.889 mm
176 °F

@Thickness 0.0350 in
UL 746
90.0 °C

@Thickness 1.40 mm
194 °F

@Thickness 0.0551 in
UL 746
90.0 °C

@Thickness 3.00 mm
194 °F

@Thickness 0.118 in
UL 746
Flammability, UL94 HB

@Thickness 0.889 mm
HB

@Thickness 0.0350 in
HB

@Thickness 1.40 mm
HB

@Thickness 0.0551 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Oxygen Index 25 %
25 %
ASTM D2863
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V

@Thickness 3.00 mm
>= 600 V

@Thickness 0.118 in
UL 746
Hot Wire Ignition, HWI 60 - 120 sec

@Thickness 3.00 mm
60 - 120 sec

@Thickness 0.118 in
UL 746
High Amp Arc Ignition, HAI 60 - 120 arcs

@Thickness 3.00 mm
60 - 120 arcs

@Thickness 0.118 in
UL 746
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F
Processing Temperature
Descriptive Properties Value Comments
Appearance Opaque