Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 503 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
Hot Wire Ignition, HWI | 7.00 - 120 sec | 7.00 - 120 sec | Average value: 34.5 sec Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL Rating PLC 1 (60-120 sec) |
Covestro Bayblend® KU2-1500 Polycarbonate + ABS Blend, Extrusion/Blow-Molding
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem 1000FV PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1010R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem 1010RV PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2110EPR PEI 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2212R PEI 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2300R PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM ATX100 PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 553 PBT+PC 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 780 PBT 40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4101 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4103 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 77-W115-B Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Uses: Connects; Grommets; Plugs; Strain ReliefsForms: Pellets Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Components Additional Information: T.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Noryl N1251 PPE+PS ECO-FLO(tm). ECO conforming, non-halogen flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2110R PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PX5379 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_PX5379 compound is a 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4011 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Europe-Africa-Middle East) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL Rating PLC 1 (60-120 sec) |
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.05 mm |
60 - 120 sec @Thickness 0.120 in |
UL PLC 1 |
Resinoid 1322 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL Rating PLC 1 (60-120 sec) |
Covestro Bayblend® FR 90 Polycarbonate + ABS Blend, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |