Teknor Apex Beetle® MD21 Nylon 6, Extrusion Grade

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer Teknor Apex Company
Trade Name Beetle®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Beetle® MD21 Nylon 6, Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: MD21 is a medium viscosity grade of nylon 6, designed for wire coating extrusion. MD21 is heavily pigment and is designed to provide good opacity even with thin coatings. It also features a lubrication system that is designed to ensure excellent adhesion between the wire and the coating - as well as optimal processing characteristics at high line speeds. MD21 is available in a range of colors - including heavy metal free options. Features: Tailored nylon 6 based compounds for coating steel wires; High opacity even in very thin coatings; Wide color range including heavy metal free options; Good Adhesion; Good Processability; Lubricated Processing Method: Extrusion Forms: Pellets Uses: Wire and Cable Applications; Wire JacketingInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Filler Content 0.00 - 25 %
0.00 - 25 %
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Strength 13.0 kV/mm

@Thickness 3.00 mm
330 kV/in

@Thickness 0.118 in
ASTM D149
Processing Properties Metric English Comments
Zone 1 250 - 300 °C
482 - 572 °F
Zone 3 250 - 300 °C
482 - 572 °F
Zone 5 250 - 300 °C
482 - 572 °F
Melt Temperature <= 300 °C
<= 572 °F
Drying Temperature 80.0 - 100 °C
176 - 212 °F
Dry Time 2 hour
2 hour
Descriptive Properties Value Comments
Appearance Colors available; Opaque