Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Chemlon® 109-18 GH Nylon 66, 18% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Teknor Apex Company
Trade Name Chemlon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Chemlon® 109-18 GH Nylon 66, 18% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: High-impact; Reinforced with 18% glass fibers; Highly toughened compound designed to improve practical toughness and ductility Features: Ductile; Good Impact Resistance; Good Toughness; Good Creep Resistance; Good Stiffness; Heat Stabilized Processing Method: Injection Molding Forms: Pellets Additive: Heat stabilizerInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 86.2 MPa
12500 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 3.72 GPa
540 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm

@Temperature 22.8 °C
2.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 221 °C
430 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 254 °C
490 °F
Descriptive Properties Value Comments
Appearance Black; Natural Color
Users viewing this material also viewed the following: