Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Flexalloy® 3500-45 Polyvinyl Chloride Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Vinyl (PVC)
Manufacturer Teknor Apex Company
Trade Name Flexalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Flexalloy® 3500-45 Polyvinyl Chloride Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
15 seconds; ASTM D2240
Tensile Strength, Yield 2.55 MPa
370 psi
100%; ASTM D412
8.48 MPa
1230 psi
ASTM D412
Elongation at Break 360 %
360 %
ASTM D412
Tear Strength, Total 599.4 N
134.8 lb (f)
Die C; ASTM D1004
Compression Set 12 %
12 %
73°F, 22 hr.; ASTM D395
57 %
57 %
158°F, 22 hr.; ASTM D395
65 %
65 %
212°F, 22 hr.; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -55.0 °C
-67.0 °F
ASTM D746
Users viewing this material also viewed the following: