Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
ASTM D2240
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB