Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.96 MPa
1300 psi
at 2% Offset; ASTM D638
ExxonMobil LD 509.48 Compounding Resin  (discontinued **)
LD 509.48 is a high melt index homopolymer resin designed to provide good processability in compounding applications.Information provided by ExxonMobil Chemical
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D638
M. Holland Company LD300 LDPE  (discontinued **)
Features: High ESCR (Stress Crack Resist.), Good Processability, Low Temp. StrengthUses: Closures, Electrical Parts, Household GoodsApprovals: FDA 21 CFR 177.1520(c) 2.2Processing Method: Injection ..
Tensile Strength, Yield 8.96 MPa

@Temperature 23.0 °C
1300 psi

@Temperature 73.4 °F
ASTM D638
Ineos T00G-00 Polypropylene Impact Copolymer
This is a fractional MFR polypropylene impact copolymer designed for the roofing membrane market. Its blend of impact resistance and flexural modulus is designed to provide an excellent balance bet..
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D638
LyondellBasell Petrothene® NA831000 Low Density Polyethylene
ApplicationsPETROTHENE NA831-000 resin exhibits high stress crack resistance and low temperature brittleness. Typical applications include housewares, containers and industrial parts. Regulatory St..
Tensile Strength, Yield 8.96 MPa
1300 psi
Elastic; ASTM D412
Multibase Multi-Flex® A 7204 LC TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Tensile Strength, Yield 8.96 MPa
1300 psi
Elastic; ASTM D412
Multibase Multi-Flex® A 7802 TPE Blk Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Tensile Strength, Yield >= 8.96 MPa
>= 1300 psi
Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7148 Fluorocarbon-Elastomer
FKM specially for oil & gas service; ED resistantInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 8.96 MPa
1300 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 7267 Ethylene-Propylene Rubber
EPDM for high temperature steam service. Also available as a Y267-Type (7267L).Information provided by Seals Eastern, Inc.
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D412
Teknor Apex APEX® 1700-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose, Low Gloss Uses-Appliance Components, Footwear, FurnitureForms-PelletsProcessing Met..
Tensile Strength, Yield 8.96 MPa
1300 psi
100%; ASTM D412
Teknor Apex APEX® 3301-80 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D412
Teknor Apex APEX® 3310-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med..
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D412
Teknor Apex APEX® 3311-55 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
Tensile Strength, Yield 8.96 MPa
1300 psi
100%; ASTM D412
Teknor Apex Flexalloy® 3501-75-NT Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe..
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D412
Teknor Apex MONPRENE® MP 2850M Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield >= 8.96 MPa
>= 1300 psi
Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7182B Fluorocarbon-Elastomer
Formulated AFLAS® high-temperature, high-pressure "sour" oil & gas service. ED resistant. Excellent acid and base resistance.Information provided by Seals Eastern, Inc.
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D412
Teknor Apex TEKBOND® MP 1723 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D412
Teknor Apex UNIPRENE® 7010-87 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 8.96 MPa

@Strain 300 %
1300 psi

@Strain 300 %
ASTM D412
Clariant OMAN698583 Thermoplastic Polyurethane, Halogen Free, Flame Retardant
Aromatic Polyether BasedData provided by Clariant Masterbatches
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D-638
Axiall 53061A Moldings & Extrusions Flexible PVC
General purpose injection molding and extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D-638
Axiall 7540 Moldings & Extrusions Flexible PVC
A high quality clear outdoor grade PVC molding and extrusion compound formulated for good UV light resistance and excellent low temperature properties.Information provided by Georgia GulfGeorgia Gul..
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D638
Multibase Multi-Flam™ 0803 LDPE NH Polyethylene
Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingInformation provided by Multibase
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D638
Aaron Industries AVPE LD 300-1 MELT 20 Virgin Polyethylene
A natural, high flow Low Density Polyethylene resin, specifically designed for high speed injection molding applications.
Tensile Strength, Yield 8.96 MPa
1300 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-3870E Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:ExtrusionPolyOne First ChoiceDisclaimer: A ther..
Tensile Strength, Yield 8.96 MPa
1300 psi
Elastic; ASTM D412
Multibase Multi-Flex® A 8103 E Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection MoldingExtrusions Information provided by Multibase
Tensile Strength, Yield 8.96 - 35.2 MPa
1300 - 5110 psi
Average value: 25.1 MPa Grade Count:200
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..
Tensile Strength, Yield 8.96 - 110 MPa
1300 - 16000 psi
Average value: 26.4 MPa Grade Count:712
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..