Teknor Apex Telcar® TL-3050 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Teknor Apex Company
Trade Name TELCAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Telcar® TL-3050 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Temperature Ratings: Wet Location: 75°C, Dry Location: 90°C Processing Method: ExtrusionInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
Tensile Strength 16.5 MPa
2400 psi
Elongation at Break 550 %
550 %
Thermal Properties Metric English Comments
Brittleness Temperature <= -50.0 °C
<= -58.0 °F
ASTM D746
Flammability, UL94 HB
HB
Oxygen Index 17 %
17 %
ASTM D2863
Users viewing this material also viewed the following: