Tipco Tipcolene® IA 933 IN - 20% Talc/Mineral Reinforced Polypropylene Copolymer, High Flow, Stiffness & Impact Strength

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® IA 933 IN - 20% Talc/Mineral Reinforced Polypropylene Copolymer, High Flow, Stiffness & Impact Strength.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Mineral Reinforced, High Stiffness, High Impact PP CopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 60
60
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break >= 35 %
>= 35 %
ASTM D638
Flexural Yield Strength 30.0 MPa
4350 psi
ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648