Total PPC 13812 Polypropylene, Heterophasic Copolymer, Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Total Atofina
Trade Name PPC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPC 13812 Polypropylene, Heterophasic Copolymer, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polypropylene PPC 13812 is a high fluidity heterophasic copolymer resin with fast nucleation.Polypropylene PPC 13812 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It has been formulated for excellent antistatic properties.Polypropylene PPC 13812 has been developed for high-speed injection molding of thin walled packaging containers and household articles.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ISO 1183
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Melt Flow 100 g/10 min

@Load 2.16 kg,
Temperature 230 °C
100 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ISO 2039-2
Flexural Modulus 1.25 GPa
181 ksi
ISO 178
Izod Impact, Notched (ISO) 3.50 kJ/m²

@Temperature -20.0 °C
1.67 ft-lb/in²

@Temperature -4.00 °F
ISO 180
7.50 kJ/m²

@Temperature 23.0 °C
3.57 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146