Total PPH 3060 Polypropylene, Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Total Atofina
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 3060 Polypropylene, Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ATOFINA Polypropylene PPH 3060 is homopolymer.ApplicationATOFINA Polypropylene PPH 3060 is characterized by a low fluidity for continuous extrusion of strapping, rope fibers and high tenacity tapes for bags. Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 1.7 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.7 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ISO 2039-2
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO 527-2
Elongation at Yield 10 %
10 %
ISO 527-2
Tensile Modulus 1.55 GPa
225 ksi
ISO 527-2
Flexural Modulus 1.45 GPa
210 ksi
ISO 527-2
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
120°C per hour; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
120°C per hour; ISO 75-2
Vicat Softening Point 87.0 °C
189 °F
50N-50°C per hour; ISO 306
152 °C
306 °F
10N-50°C per hour; ISO 306