Material Notes:
Fina’s new HIGH PERFORMANCE injection molding gradeBalanced Properties - Fina 3727WZ strikes an optimum balance between excellent mechanical properties (tensile, flex and impact) and processability making it a superior molding grade for cap and closure applications.Impact Strength - Fina 3727WZ offers improved impact strength.Nucleation - Fina 3727WZ is formulated to provide fast cycle time and improve contact clarity in thin wall multi-cavity molds.Antistat - Fina 3727WZ contains an antistat to help protect molded parts from dust accumulation.FDA - Fina 3727WZ complies with all applicable FDA regulations for food contact applications.Recommended Application - Fina 3727WZ is recommended for large thin wall parts, caps and closures.Processing - Fina 3727WZ resin processes on conventional injection molding equipment with typical melt temperatures of 390-450°F (200-232°C).Data provided by the manufacturer, Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238L
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 33.1 MPa
4800 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Modulus of Elasticity 1.24 GPa
180 ksi
ASTM D638
Flexural Modulus 1.03 GPa
149 ksi
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256A
Impact Test 21.6 J

@Thickness 3.17 mm
15.9 ft-lb

@Thickness 0.125 in
Drop Impact, plaques. Fina API test
Thermal Properties Metric English Comments
Melting Point 158 °C
316 °F
DSC
Vicat Softening Point 140 °C
284 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 200 - 232 °C
392 - 450 °F
Injection