Modulus of Elasticity 1.24 - 2.30 GPa
180 - 334 ksi
Average value: 1.65 GPa Grade Count:8
Overview of materials for Nylon 12, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Modulus of Elasticity 1.24 GPa
180 ksi
ASTM D638
Total PPH 3727WZ Polypropylene, Injection Molding Grade
Fina’s new HIGH PERFORMANCE injection molding gradeBalanced Properties - Fina 3727WZ strikes an optimum balance between excellent mechanical properties (tensile, flex and impact) and processability..
Modulus of Elasticity 1.24 GPa
180 ksi
ASTM D638
Total PPR 7525MZ Polypropylene, Injection Molding Grade
Clarified random copolymer for injection moldingClarity - FINA 7525MZ exhibits superior clarity in molded parts.Impact - FINA 7525MZ produces molded parts with improved impact compared with parts mo..